Views: 2422
I am having problems with a product we receive from our over...
- Mar 28, 2007
by
AMelara
Hi A,
Your subject is black solder, but you decrribe the ...
- Mar 28, 2007
by
Real Chunks
It should only be a visual thing. What may be happening is t...
- Mar 28, 2007
by
PeteC
solder joints are dull on the bottom, and surprisingly, dark...
- Mar 28, 2007
by
AMelara
Unfortunately, the facility overseas does not have a profile...
- Mar 28, 2007
by
AMelara
They were run with dross inhibitor in the pot.
...
- Mar 28, 2007
by
Dr Shocker