Hi all, What stencil aperture designs do you use for 0402... - Apr 12, 2007 by aj
There have been many designs of apertures for 0402, round, h... - Apr 12, 2007 by PeteC
Hi aj, Pete is right, there are several variables that ca... - Apr 12, 2007 by Real Chunks
the footprint is IPC standard which I have found to be less ... - Apr 14, 2007 by aj
Tombstone head and a graveyard mind. I would not recommend 1... - Apr 16, 2007 by PeteC
"Although some lead-free pastes performed adequately and new... - Apr 16, 2007 by davef
Our experience with leaded paste and SAC305, for 0402's, has... - Apr 17, 2007 by Dback
Hi, Can you advise the footprint dimensions used on the P... - Apr 18, 2007 by
Yes we can (at least show something that work for us) but he... - Apr 21, 2007 by Mika
If the PCB you are using is a HASL pad finish and is a leade... - Apr 24, 2007 by Chris1963
Hi All, Thanks for all the replies. I went with 1:1 (E... - Apr 25, 2007 by aj