I am using a Novastar 12S solder wave with Kester water solu... - May 05, 2007 by jmabie
Try to slow down your conveyor speed. This reduces contact ... - May 07, 2007 by Dirk Nuendyke
Hi Jerry, I bet you have dross build up on your wave. Ar... - May 07, 2007 by Real Chunks
How much flux are you putting on the board when using your f... - May 07, 2007 by davef
The spray bottle puts more flux on the board but I am not su... - May 07, 2007 by jmabie
Are the pallets hot and killing the foam head as they pass o... - May 07, 2007 by BLT Circuit Services Ltd
4 Fluxer Operation 4.1 Set-Up and Check-Out the Fluxer 4... - May 07, 2007 by davef
Flux foam is not affected by board or pallot. This wave ... - May 07, 2007 by jmabie
Just as I thought earlier, you have a stagnant wave. You ... - May 07, 2007 by Real Chunks
Jerry, If you�re sure your board has sufficient flux it m... - May 07, 2007 by Patrick Bruneel
I have the option of increasing the wave pump but when I do ... - May 07, 2007 by jmabie
Jerry, At the end of the article in the link you will see... - May 07, 2007 by Patrick Bruneel
Jerry, In your initial post you give 260C as solder pot t... - May 07, 2007 by Patrick Bruneel
Thank you all for your help. I will fire up the wave again F... - May 07, 2007 by jmabie
What is a smart way to determine that the solder in the wave... - May 07, 2007 by davef
Dave, There is not really a �smart� or scientific way to ... - May 07, 2007 by Patrick Bruneel
Patrick I think peelback mechanics is more important than wa... - May 07, 2007 by Dirk Nuendyke
what type of preheater does the novastar use and what temp. ... - May 07, 2007 by SEB
radiant heat. 137c The hollis was a great machine. The on... - May 07, 2007 by jmabie
Use the good old glass plate? ... - May 08, 2007 by Loco
Hi Loco, Good point!! The good old glass plate works jus... - May 08, 2007 by Patrick Bruneel
Hi Jerry, Today is Friday and I assume you fired up your ... - May 11, 2007 by Patrick Bruneel
Novastar is JUNK, that is why you cannot get repeatable resu... - May 11, 2007 by ml
Authough your response is harsh I tend to agree with you. I ... - May 11, 2007 by jmabie
Can't do much better than Electrovert. ... - May 14, 2007 by Real Chunks
Agreed, I just bought a Electrovert Vectra Elite and have be... - May 14, 2007 by jdumont
What did it cost ? ... - May 14, 2007 by jmabie
You can get a nice used electrovert in your budget. ... - May 14, 2007 by RDR
We got a good deal on ours for around $100K new with not man... - May 16, 2007 by jdumont
Since your budget is between 25 and 30K I would say you have... - May 17, 2007 by Bryan