Re: 63/37 paste reflow
Is there a standard reccomended ti...
- May 09, 2007
by
Jim Z
30 to 90 seconds TAL is typical.
...
- May 10, 2007
by
PeteC
There is no standard for time above liquidus. It is describ...
- May 10, 2007
by
davef
I have been TAL around 45 to 90 seconds. I prefer the longe...
- May 18, 2007
by
Ed Faranda
TAL Too Long - dull solder joints, dewetting.
TAL Too Short...
- May 25, 2007
by
mfgengr
Look here: ...