We have not processed very much 0402 size components in the ...
- Jun 15, 2007
by
Prologic Engineering Inc
Good morning,
5mil stencil or less would be appropriate. ...
- Jun 18, 2007
by
Hypnotia
Agreed.
...
- Jun 18, 2007
by
Sr. Tech
5mil should work fine. Some stencil manufacturers charge mo...
- Jun 18, 2007
by
dyoungquist
5 mil is perfect for 0402's.
If you are printing SnPb sol...
- Jun 21, 2007
by
Chris1963
5mil works great. Just make sure that you screen alignment ...
- Jun 22, 2007
by
Ed Faranda
5 mil will treat you just fine. Do some research on stencil...
- Jun 27, 2007
by
SMT Frog
Laser cut 0.13mm stencil thicknes works great for us.
BTW, ...
- Jun 28, 2007
by
Mika