I want to get a collective opinion from the forum... I was ... - Aug 23, 2007 by garyr
Water soluable fluxes are quite hydroscopic. If you keep RH... - Aug 23, 2007 by davef
Solder balls with wave soldering can have different causes. ... - Aug 24, 2007 by Joris Groot Koerkamp
I agree with Joris. But to add to his comment, the type of ... - Aug 24, 2007 by Hussman
What about when using noclean and alcohol based fluxes? Cou... - Aug 24, 2007 by garyr
I would say no, unless your machine is in extremeconditions.... - Aug 24, 2007 by Hussman
This is what I was thinking, but I am being beat up pretty b... - Aug 28, 2007 by garyr