Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
We are seeing a white, powdery residue following the Wave pr... - Mar 02, 2001 by Gary Kemp
Is this after wave or wash? Its too bad the archives are gon... - Mar 02, 2001 by Travis Slaughter
This happens to be after the water wash process. These are ... - Mar 02, 2001 by Gary Kemp
If the thinner you are using is 4662 and the correct amounts... - Mar 02, 2001 by Travis Slaughter
I had confused by same problem, the reason I found is the in... - Mar 03, 2001 by Wister
When you say all over the board, please give more detail. Wh... - Mar 05, 2001 by davef
I have experience to the Kester 2331 water soluble flux long... - Mar 06, 2001 by Dason C