Views: 4203
What are you using? I'm having a tough time finding somethin...
- Nov 01, 2007
by
Steve Thomas
Here's what I use:
Sn10/Pb90, 268C-302C
...
- Nov 01, 2007
by
PeteC
That might be the stuff. I think what baffles me is that it ...
- Nov 01, 2007
by
Steve Thomas
Steve, your best solderer in your shop will know that this a...
- Nov 02, 2007
by
Dirk Nuendyke
I also use a very high lead content solder for this. Its awf...
- Nov 02, 2007
by
jdumont
I always do tc attachment myself. I need these people not to...
- Nov 05, 2007
by
Steve Thomas
Radio Shack "Lead-free" Sn96Ag4 480�F
...
- Nov 05, 2007
by
davef