our boards have many smd pads that has vias under them so wh...
- Nov 05, 2007
by
omid_juve
Hi,
We are also interested in this, and I have heard you ...
- Nov 05, 2007
by
Grant
Hi,
We have had this before - yes they can be plugged and...
- Nov 05, 2007
by
aj
Of course if you are an OEM you could go back to your design...
- Nov 09, 2007
by
devajj
Hi,
What is this unacceptable? Designed the PCB is much e...
- Nov 13, 2007
by
Grant
For the simple fact that the via in the middle of the pad ca...
- Nov 13, 2007
by
kpm
From a manufacturing standpoint, this isn't very nice. Vias...
- Nov 13, 2007
by
robgd3
Hi,
What size via's are you guys seeing, as the ones in o...
- Nov 13, 2007
by
Grant
I had one project with micro-vias in 0805 and larger pads, w...
- Nov 14, 2007
by
robgd3
Hi,
Those via's sure do sound large, and I think the desi...
- Nov 14, 2007
by
Grant
I do think that the designer goofed, and used too large vias...
- Nov 15, 2007
by
robgd3
...
- Nov 20, 2007
by
Matt Kehoe
In my past experience, having via's under or attached to SMD...
- Nov 20, 2007
by
Kelcatzeye
From info I have been told from design standpoint, via in pa...
- Nov 21, 2007
by
josh
Question: We have an issue right know on a prototype batch w...
- Nov 23, 2007
by
Mika
There a several things you can do to prevent the solder wick...
- Nov 23, 2007
by
davef
Thanks a'lot Dave F, We will look into this as soon as poss...
- Nov 23, 2007
by
Mika
Hi DaveF, I had a short look into the
Nr1. IMPACT OF MICRO...
- Nov 24, 2007
by
Mika