Does anyone have experience with automated Laser soldering e...
- Jan 04, 2008
by
adlsmt
I have seen the application with hot-bar soldering machines ...
- Jan 07, 2008
by
PeteC
OK, I'll venture to ask..... why not use a reflow oven. Not...
- Jan 07, 2008
by
Real Chunks
I agree with Chunks! Why consider laser sodlering when u can...
- Jan 07, 2008
by
fsw
The clear plastic packaging for LEDs is a LOT softer thermop...
- Jan 07, 2008
by
jmelson
I solder LEDs everyday from 0402 sizes on up. I work for an...
- Jan 09, 2008
by
Flipit
Can you tell me what LED's you are wanting to use and what s...
- Jan 14, 2008
by
QMSI
The reason we are using laser rather reflow is because the O...
- Jan 18, 2008
by
adlsmt
Craig, ...
- Jan 18, 2008
by
John Smith
Sweeet!
...
- Feb 08, 2008
by
Stockley