Looking for some opinions on what the best, readily availabl... - Jan 10, 2008 by jdumont
Hi JD, We use the OM-310 NC for most of our lead free wor... - Jan 10, 2008 by jdengler
Thanks for the reply.. May foam eh? We actually clean some o... - Jan 10, 2008 by jdumont
You may want to ask Zestron to be sure. We have a batch cle... - Jan 10, 2008 by jdengler
Yes thats always an awful site isnt it? It used to happen to... - Jan 10, 2008 by jdumont
We too are trialling WS819 with SAC305 alloy. The foaming in... - Jan 15, 2008 by Pete B
Stay far away from the WS619 paste. It is a nightmare to get... - Jan 17, 2008 by dman97