Hi
If I have an assembly where the solder joints are suf...
- Jan 16, 2008
by
Adam
In general, they certainly can be touched-up. I don't know ...
- Jan 16, 2008
by
robgd3
As Rob says, blowholes and pinholes are process indicators. ...
- Jan 16, 2008
by
davef