Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Anyone doing a print-dispense-place-reflow process? I've ne... - Mar 13, 2001 by Steve Thomas
Check Bob Willis' site. He calls this Single Side Multipass... - Mar 14, 2001 by davef
Some thing to watch out for is the cure spec for the adhesiv... - Mar 14, 2001 by Michael Parker
Mike makes a very good [ no, make that excellent!!!] point a... - Mar 14, 2001 by davef
Like I said, I would only try this if I had some sort of rea... - Mar 15, 2001 by Steve Thomas
That makes us almost even, Dave. I have a hard time believi... - Mar 15, 2001 by Steve Thomas
Don�t be afraid of the more standard doubles sided mixed pro... - Mar 15, 2001 by Travis Slaughter
The only way I know of waving the bottom side with SMT parts... - Mar 15, 2001 by Michael Parker
Like I said it was only a rumor I heard but intrigued me eno... - Mar 15, 2001 by Travis Slaughter
Wazis havin' "a hard time believing half of what you say"? ... - Mar 15, 2001 by davef
Shadowing sounds about right to me also. Really dicey experi... - Mar 16, 2001 by Michael Parker
We screen print epoxy adhesive, place components then run th... - Mar 16, 2001 by
That's what we do also. It's the "print, dispense" sequence... - Mar 16, 2001 by davef
Steve, I did this several years ago on a terribly designed ... - Mar 16, 2001 by Frank