Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6090
Hello. We have currently a big problem with our Reflow owen... - Jan 31, 2008 by Jola
My first thought is that your roof exhaust blower is dead an... - Jan 31, 2008 by Steve Thomas
Hi. There is no problem with the exhaust system and the owe... - Feb 01, 2008 by Jola
Hello, If I do understand it correct, the dust in your ov... - Feb 01, 2008 by Lozie
Its most likely flux residue from your paste. This is normal... - Feb 01, 2008 by Sr. Tech
Thanks for your replys but I can't figure out why this probl... - Feb 04, 2008 by Jola
Sure looks like flux residue to me and I don't know how your... - Feb 04, 2008 by Steve Thomas
Recently I have been hearing and see this excess flux residu... - Mar 04, 2008 by Gary Z.
An industry issue??? Sounds more like another ROHS issue to... - Mar 04, 2008 by Loco
Hi. Thanks for your replies and your inputs in this. Regar... - Mar 04, 2008 by Jola
What are you profile temperatures? I wonder if you're not r... - Mar 04, 2008 by Real Chunks
Our profile tempatures in the owen is: Preheat 6 zoones 135... - Mar 04, 2008 by Jola
If your oven has the flux collection unit just like the Tamu... - Mar 11, 2008 by Portadz