Anyone knows why BGA fell off sometimes from the board? I wa... - Feb 14, 2008 by jo
How many fell off out of your entire lot? What was the solde... - Feb 14, 2008 by jdumont
There was hardly a dropped component or components under the... - Feb 14, 2008 by aj
Questions are: * Do the BGA pads on the board take solder w... - Feb 14, 2008 by davef
That is bizarre. I would have to say that you need to do a t... - Feb 14, 2008 by operator
Thanks for the comments and advice. The rest of the componen... - Feb 15, 2008 by jo
Creating a sound tin nickel intermetalic takes a bit more en... - Feb 15, 2008 by SteveK
4 days seems a lot. You could be losing flux activation cau... - Feb 18, 2008 by Loco