Hi All, I have some question about expired solder paste. ... - Apr 03, 2008 by AlexS
Potential impacts of using expired solder paste are [Univers... - Apr 03, 2008 by davef
All of what Dave says is spot on. I suspect that the most li... - Apr 04, 2008 by Steve Thomas
Define "expired" though... 1 week? 6 weeks? 1 month? 6 mo... - Apr 04, 2008 by Dirk Nuendyke
Flux seperation is a common problem observed due to expirati... - Apr 04, 2008 by Wave
Thanks for the reply. Just one more question. If there is... - Apr 04, 2008 by AlexS
can we use the expired solder paste and put in a solder pot ... - Apr 07, 2008 by kircchoffs
Yes you can, although we don't think it's a good idea. Look ... - Apr 07, 2008 by davef