I have a small board with some chips and 2 connectors (1 lar...
- Apr 18, 2008
by
sueph
Do you have a picture? SMTNet HAS the technology now to pos...
- Apr 18, 2008
by
Dirk Nuendyke
That you have 'grainy' solder only at the ends of the connec...
- Apr 21, 2008
by
davef
"Disturbed" usually means some form of movement. I would th...
- Apr 21, 2008
by
Real Chunks
Profiling can't happen outside of North Avenue.
...
- Apr 21, 2008
by
Peter Gibbons