would anybody guide me about soldering and unsoldering the B... - May 17, 2008 by azimi789
You should set the temperature at liquidus point of the sold... - May 19, 2008 by davef
I just set that as you said, but the component doesn't stick... - May 20, 2008 by azimi789
Did you get the solder to the temperature? Determine the tem... - May 21, 2008 by davef
I found out that the light is not heterogeneous, i am trying... - May 22, 2008 by azimi789
No, absolutely not. The BGA balls should collaps by theirse... - May 22, 2008 by Loco