Does anybody use a paste mixer in their shop? I am looking ... - Jun 04, 2008 by Dirk Nuendyke
yes and yes it has. also it has reduced the time of paste pr... - Jun 04, 2008 by Cattle
We have hand mixed several million grams of solder paste in ... - Jun 05, 2008 by Sr. Tech
Ours run out of control and caght the paste on fire! I gues... - Jun 06, 2008 by Dr Shocker
Every paste supplier I've talked to has recommended against ... - Jun 09, 2008 by ScottE