I am using TopazX2, placing 0603 caps with #72 FNC nozzles.
...
- Jun 16, 2008
by
DucHoang
Could it be from a dirty stencil, rather than from the pick ...
- Jun 17, 2008
by
robgd3
You need to adjust the air kiss. The machine blows a slight ...
- Jun 17, 2008
by
dwelch123
"The machine blows a slight amount of air after placement an...
- Jun 17, 2008
by
DucHoang
vo^ cai' tab pick vacuum% set at 30 and tab mount vacuum % s...
- Jun 18, 2008
by
GEM
You're barking up the wrong tree. Solder "splashes" are gen...
- Jun 18, 2008
by
Real Chunks
service manual for topaz-xII chapter 15
set vacuum chapter...
- Jun 18, 2008
by
GEM
Hi Russ/Dave/Allen,
Is the solder splash and solder ball ...
- Jul 22, 2009
by