Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5166
Hi all,
What should the typical gold thickness be on ENIG...
- Jul 10, 2008
by
aj
Search the fine SMTnet Archives to find threads like: ...
- Jul 10, 2008
by
davef
Thanks Dave,
IPC-6012 states min at 0.05um.
Has this b...
- Jul 11, 2008
by
aj
0.05 um => 2 uinch, right?
Here is the revision level for...
- Jul 11, 2008
by
davef
Hi Dave,
Yes that is correct.
I had a XRF carried out ...
- Jul 11, 2008
by
aj
Hi Aj,
Recommended Immersion gold thickness would be 3-5 ...
- Jul 15, 2008
by
BoardHouse
Please look up ...
- Jul 28, 2008
by
Mark