Hello everyone,
I have too much solder balls in my smt pr...
- Jul 15, 2008
by
gabriella
Can you describe your solder balls...mid-chip solder balls, ...
- Jul 15, 2008
by
Steve Thomas
I would say the balls are aminly on passive parts in the mid...
- Jul 17, 2008
by
gabriella
To quote a regular here, "Are you sure your washer is set up...
- Jul 17, 2008
by
Steve Thomas
"Are you sure your washer is set up correctly?"
Now, tha...
- Jul 17, 2008
by
davef
Which type?
* Solder beads (mid-chip solder balls, attached...
- Jul 17, 2008
by
davef
Try using a homeplate design on your stencils.
Works eve...
- Jul 18, 2008
by
Real Chunks
I think Real Chunks has your answer home plat or reverse
ho...
- Jul 18, 2008
by
WRONGWAY
Thats it.
6 mils works great with a 10% reduction.
We ...
- Jul 18, 2008
by
garyr
We have created a new online free database on process defect...
- Jul 26, 2008
by
Bob Willis
Your problem is being caused by to much paste being printed....
- Jul 28, 2008
by
Mark
Hello everyone,
thanks for the feedback. Now I am sure it...
- Jul 28, 2008
by
gabriella
Be careful of just reducing your aps. Too much can cause to...
- Jul 28, 2008
by
Real Chunks