How many times do you measure your oven's profile? I have se... - Jul 15, 2008 by Armando
Armynski, You should do a Cpk study to baseline how capab... - Jul 16, 2008 by Dirk Nuendyke
We use a "gold" board to verify the performance of the oven.... - Jul 16, 2008 by mrmaint
> Armynski, > > You should do a Cpk study to &... - Jul 16, 2008 by Armando
With our last two ovens (Heller and now BTU) spanning the pa... - Jul 17, 2008 by jdumont
JDumont is right on the money. With today's modern reflow o... - Jul 17, 2008 by Dirk Nuendyke
....but try to tell that to an ISO/AS9100/Mil/Avionics type ... - Jul 17, 2008 by jdumont