What chemical is everybody using in their wave solder finger...
- Jul 29, 2008
by
Jeff
IPA is a fire hazard. Be sure your fire extinguishers are ch...
- Jul 29, 2008
by
davef
Zestron's Vigon RC-101...Good with no clean
...
- Jul 30, 2008
by
garyr
You may want to try C8502 from Kyzen Corp. I use it on our t...
- Jul 30, 2008
by
George
We use Axarel 2200 as recomended by Vitronics Soltec, which ...
- Jul 31, 2008
by
Jon Hall
Jon,
Does Axarel 2200 leave minimal residue or clumps on th...
- Jul 31, 2008
by
Dirk Nuendyke
Try Zestron Vigon RC 101. This mixes with tap water. Electro...
- Aug 01, 2008
by
PeteC