We had experienced two (2) A BGA which fail (detached) off t... - Aug 11, 2008 by Eyal
Sounds like solder is not taking to the pads of the BGA inte... - Aug 11, 2008 by davef
I assume you mean the balls of the BGA, not pads (laugh it u... - Aug 11, 2008 by Real Chunks
> I assume you mean the balls of the BGA, not pads >... - Aug 11, 2008 by Eyal
RoHS BGA. No lead in it. ... - Aug 11, 2008 by Real Chunks
> RoHS BGA. No lead in it. > RoHS BGA. No lead i... - Aug 11, 2008 by Eyal
Your defect may be possibly due to black pads, although it i... - Aug 11, 2008 by Wave
Then your profile is way off. You need a t-couple mounted u... - Aug 11, 2008 by Real Chunks