hai, we r using type 4 solder paste in our pcb assembly pro... - Sep 06, 2008 by ramesh.r
We can't help but wonder: * What are the measured temperatu... - Sep 06, 2008 by davef
Does look like a poor reflow profile needs to be hotter, is ... - Sep 07, 2008 by BLT Circuit Services Ltd
1.The Temperature on the pad is 247.C & also it is an lead f... - Sep 08, 2008 by ramesh.r
Here we go with another "solderability problem". How do you... - Sep 08, 2008 by Vlad
Of the six pads in the picture, which are the two that are u... - Sep 08, 2008 by davef
God..... give it a rest. ... - Sep 09, 2008 by WaveMasterLarry
I wish i saw at least one problem posted here being solved b... - Sep 09, 2008 by Vlad
Perhaps people are solving their problems by turning knobs a... - Sep 09, 2008 by Steve Thomas
May be you right, but I spend a lot of time on Technet (a si... - Sep 09, 2008 by Vlad
In the real world where I work, I turn knobs (really key boa... - Sep 10, 2008 by Real Chunks
And I bet you are not alone :-). All I'm trying to say is th... - Sep 10, 2008 by Vlad
You missed my point. People often don't find the need to ... - Sep 10, 2008 by Steve Thomas
Amen to that!!! When I was still on the production floor ... - Sep 10, 2008 by Patrick Bruneel
True words of wisdom. Production managers need product out ... - Sep 10, 2008 by garyr
Am glad we got that straight There is a big difference be... - Sep 10, 2008 by Patrick Bruneel
Dave, I don't think you will get a response in the mean t... - Sep 10, 2008 by Patrick Bruneel
No arguments there. I 100% agree that quality engineers can ... - Sep 10, 2008 by Vlad
"I 100% agree that quality engineers can and do solve a lot ... - Sep 10, 2008 by Steve Thomas
At the risk of painting with too broad a brush: QEs are lik... - Sep 10, 2008 by ScottE
"When we solving a problem we have to be absolutely sure it'... - Sep 10, 2008 by Steve Thomas
To me it speaks about teh quality of the engineers. I[ve see... - Sep 10, 2008 by Vlad
And doing analysis you are NOT changing things. Vlad ... - Sep 10, 2008 by Vlad
ISSG, I didn't see you mention anything with respect to prof... - Sep 11, 2008 by Steve Thomas
Hi, I had similar problem a while back. Diagnosis was ... - Sep 11, 2008 by aj
YES! Reflow Profile knobs have been verified. ... - Sep 11, 2008 by InSourceSolderGuy
I'm curious how many knobs have left to be turn? :-) Isn't ... - Sep 11, 2008 by Vlad