Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2600
What is this? I thought 63sn 37pb was the norm. What is with...
- Sep 09, 2008
by
Logannsan
Silver (Ag). It's a typical composition
Regards,
Vlad
...
- Sep 09, 2008
by
Vlad
Logannsan,
you may want to check into this a little more ...
- Sep 09, 2008
by
BoardHouse
As far as I know, they rarely do it with Pb-bassed solders. ...
- Sep 09, 2008
by
Vlad
Actually it's not rare. I use several pastes from various m...
- Sep 10, 2008
by
Real Chunks
Isn't that the non-eutectic one that provides the pasty phas...
- Sep 10, 2008
by
Steve Thomas
That is exactly what I said. Rarely belongs to Cu or Ni :-)
...
- Sep 10, 2008
by
Vlad
The 2 % is Ag.It is added to prevent leaching silver from th...
- Sep 11, 2008
by
Mark