Hi Has anyone experienced laminateand BGA cracking on ENI... - Sep 15, 2008 by Adam
Hi Adam, Since you don't see any cracking right after re-... - Sep 15, 2008 by Vlad
Would you attach pix of the sections? ... - Sep 16, 2008 by davef
Adam, Most leadfree components can handle only 260C. Whe... - Sep 17, 2008 by yam6rider
Hi Please see attachment Adam ... - Sep 18, 2008 by Adam
It looks "normal" for that type of failure Vlad ... - Sep 18, 2008 by Vlad
Hi Vlad Please explain "Normal" ? Adam ... - Sep 18, 2008 by Adam
Any crack in laminate caused by excessive flexure would look... - Sep 18, 2008 by Vlad
Ditto, we just went through this with a customer "fitting" o... - Sep 18, 2008 by Jon W.