I had a vendor change thier lead finish from tin/lead to a S...
- Sep 16, 2008
by
Trynders
Well, typical content of Pb in Sn/Pb polating is a few perce...
- Sep 16, 2008
by
Vlad
Yes, this scenario is fine. However, BGAs are a different s...
- Sep 16, 2008
by
Dirk Nuendyke
Well, as we are talking about lead finish, I don't think the...
- Sep 16, 2008
by
Vlad
Vlad, yes, he made no mention of a BGA, but I thought I'd ju...
- Sep 16, 2008
by
Dirk Nuendyke
Thanks for the response! I thought is was odd the component ...
- Sep 16, 2008
by
Trynders
Even BGA may be no braner if it's done properly :-) I had a ...
- Sep 16, 2008
by
Vlad
There is one thing you should keep in mind, though. It's bet...
- Sep 17, 2008