I have a job that requires a minimum of 3% lead in all compo...
- Oct 07, 2008
by
Doug Philbrick
If at all possible buy parts with 3% min. lead on the termin...
- Oct 07, 2008
by
MikeS
Why not build with a leaded paste or solder pot? You'll hav...
- Oct 09, 2008
by
Hussman