We have 8 layer HASL PCB. We saw molten solder blobs / balls... - Oct 23, 2008 by Worldwide Solutions
Good Morning WS, If you experieced the solder balls after... - Oct 24, 2008 by CL
So you passed a BARE board thru the oven and got solder ball... - Oct 27, 2008 by Hussman
solder ball was caused by hasl process not reflow. seen befo... - Oct 30, 2008 by BLT Circuit Services Ltd
I have to agree with Patrick here. This image appears to sho... - Nov 04, 2008 by SMT Tech