Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3150
We are encountering similar problem as yesterdays posting, w... - Jan 16, 2009 by Kuru
HI , A LOT OF SIMILAR ISSUES WERE DISCUSSED LATELY. MOST ... - Jan 16, 2009 by emil
Had the same problem with boards from China. Try using Scot... - Jan 16, 2009 by Real Chunks
Thanks, we tried using some very fine sand paper and did imp... - Jan 16, 2009 by Kuru
i would not try to chemically clean the finish, you would ju... - Jan 16, 2009 by BoardHouse
try making your boards in the USA. There's better QC, and if... - Jan 22, 2009 by jeffcali
Hi Jeff, Unfortunately there is just as many bad shops in... - Jan 22, 2009 by BoardHouse