what is the impact if a solder paste is used after 24 hours ...
- Jan 17, 2009
by
praveen
We're not sure of the condition of your solder paste. So, af...
- Jan 18, 2009
by
davef
Depends on the solder paste.
If it has been on the stencil ...
- Jan 20, 2009
by
MrDif
MrDif: You don't add fresh paste to used paste? We add fresh...
- Jan 20, 2009
by
davef
Sorry if that sentence there was not really clear.