We have been having problems with proper wetting when runnin... - Mar 27, 2009 by Quadraphonic
Let me be the first to suggest; Get a better oven. 5 zones... - Mar 27, 2009 by Stephen
Check with your paste manufacturer for a recommended baselin... - Mar 27, 2009 by robgd3
thanks for the responses. Went to Kester. Better now. ... - Mar 31, 2009 by Quadraphonic
Hard to beleive anything from Kester these days would help. ... - Apr 03, 2009 by EMS-Engineer
HI !!! We have the same oven! and yes profiling is hard, ... - Apr 12, 2009 by Armando_Gomez
That would be great Armando, thanks. Also, what changes mig... - Apr 13, 2009 by Quadraphonic