Views: 4841
I have a VJE Summit 750 Rework machine... I don't think tha...
- Apr 03, 2009
by
Ed Faranda
Cause: Solder between the pad and the BGA on the pads being ...
- Apr 04, 2009
by
davef
I agree the longer soak will help provided you are not apply...
- Apr 06, 2009
by
C111
Here are some pictures of the part.
I created a profile ...
- Apr 06, 2009
by
Ed Faranda
I would use almost the same profile you use when putting the...
- Apr 08, 2009
by
Steve
Another suggestion for it. Baking the whole boards before re...
- Apr 09, 2009
by
fowlerchang
Well, I did manage to solve this problem. I lowered the max...
- Apr 09, 2009
by