Hi,
I am trying to reduce some 0402 cap tombstones.
Th...
- Apr 15, 2009
by
rtmitchell
I've had some luck with longer soak. Of course that was on a...
- Apr 16, 2009
by
kpm
We know virtually nothing about your process, but here's som...
- Apr 16, 2009
by
davef
have you try to change the stencil apertures to another figu...
- Apr 17, 2009
by
Armando_Gomez
Hi, follow up,
Thanks to everyone that responded.
We f...
- Apr 17, 2009
by
rtmitchell
I have a solution.... contact me by mail
Vapor phase gives ...
- Apr 18, 2009
by
Alfred Moran
Low tombstone pastes have been around for 8-10 years. Talk t...
- Apr 18, 2009
by
davef
I like this suggestion the best as a "band aid", check out s...
- Apr 18, 2009
by
Bill West
Home plate design is great for avoiding beads and tombstonin...
- Apr 21, 2009
by
Viking
TOMBSTONING OF 0402 AND 0201 COMPONENTS: "A STUDY EXAMINING ...
- Apr 24, 2009
by