Hello All We are going to run our frist 0402 parts soon. do... - Jul 01, 2009 by WRONGWAY
You can use regular paste and a .005 stencil will help reduc... - Jul 01, 2009 by dwelch123
For 0402s we use type 3 paste. We have .006 and .005 stenci... - Jul 02, 2009 by dyoungquist
Thanks for the replies guys they will help me out. this web... - Jul 02, 2009 by WRONGWAY