Hi folks!
We seen to be getting Black Pad phenomenon, not...
- Jul 09, 2009
by
Jon Hall
We can't tell from your picture that you have black pad, but...
- Jul 09, 2009
by
davef
Yes it is very usual problem with BGA components, and you ca...
- Jul 22, 2009
by
Sasha