Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5927
does anyone knows how to calculate a correct fluxer traverse...
- Sep 25, 2009
by
kircchoffs
Here's a stab at it...
Decide on how much overlap you nee...
- Sep 29, 2009
by
MikeS
We don't know of a calculation, but we run ours as fast as w...
- Sep 29, 2009
by
davef
I never calculate it when I setup a profile...I have a feel ...
- Sep 30, 2009
by
MikeS
Find: Spray Fluxing for Pb-Free Wave Soldering; S Arora & S ...
- Sep 30, 2009
by
davef