Hi all,
I'm today looking for adhesive specifications on ...
- Nov 03, 2009
by
CooLepse
Search the finee SMTnet Archives for previous posts on the t...
- Nov 03, 2009
by
davef
Hi Davef,
I have already checked the SMTnet archives but ...
- Nov 04, 2009
by
CooLepse
There may be supplier guidelines or accepted practice, but t...
- Nov 04, 2009
by
davef
For 1206 SHEAR VALUE REQUIRED IS 30 TO 70 gmfcm.
please tel...
- Nov 04, 2009
by
SMT Process Engineer
Hi Rajeshmara,
Mail sent with the datasheet of the glue w...
- Nov 05, 2009
by
CooLepse
In a previous job, we had torque off requirements for differ...
- Nov 05, 2009
by
Lynn Norman
Up!
Thanks anyway for your answer Lynn.
But I'm still ...
- Nov 12, 2009
by
CooLepse
Hi dave,
Sorry to hi-jack the tread a bit, but,we are exp...
- Nov 13, 2009
by
Loco
Loco
[snip]
"The print mode is another consideration. Pr...
- Nov 13, 2009
by
davef
Thanks dave,
We have our problem down to the stencil (pri...
- Nov 19, 2009
by
Loco
The design of the opening apertures for the glue stencil and...
- Nov 25, 2009
by
Heny