I need to profile a single sided board thats width is less t... - Dec 14, 2009 by jammm
Yes, there will be a difference. When the board is on the r... - Dec 14, 2009 by dyoungquist
I have moved golden boards from chains to mesh as I got tire... - Dec 15, 2009 by SWAG
jamm, As with the other answers you've received, I agree th... - Dec 18, 2009 by GAZupfer