Is it possible to reflow leaded or lead-free solder paste on... - Dec 23, 2009 by SteveO
We doubt that you can successfully solder to chrome ... - Dec 23, 2009 by davef
Can you etch where you want to solder to? But you would nee... - Dec 23, 2009 by Stephen
Thanks for the replies. I haven't soldered to a chrome plat... - Dec 23, 2009 by SteveO
You can weld (spot) to chrome. Maybe you could weld a nickel... - Dec 24, 2009 by isd.jww
isd.jww: First, the original poster is talking about pads... - Dec 24, 2009 by davef
That's not going to work in this case. The substrate has ve... - Dec 28, 2009 by SteveO
How about silver epoxy? Could you use a PnP with a dispenser... - Dec 28, 2009 by isd.jww