Looking for methods for detecting BGA microcracks without cr...
- Feb 08, 2010
by
Woodsmt
We believe that neither xray nor SAM will provide satisfacto...
- Feb 08, 2010
by
davef
Dave,
I agree totally, but dye-and-pry should also be p...
- Feb 08, 2010
by
glennr
Thanks Dave and Glenn,
I have setteled on Dye for the des...
- Feb 08, 2010
by
Woodsmt
Woody: Consider using test BGA with no chip in, but daisy ch...
- Feb 08, 2010
by
davef
Woody,
Daisy chain packages are definitely needed, but ...
- Feb 08, 2010
by
glennr
Daisy chained parts and impedence testing were my original r...
- Feb 10, 2010
by
Woodsmt
It's OK to have the daisychain done in the interposer rather...
- Feb 11, 2010
by
ScottE