Is there any harm in washing SMT soldered with NoClean paste...
- Feb 23, 2010
by
Vince
There should be no problem. Recognize that the residue of s...
- Feb 23, 2010
by
davef
Davef is right on as usual. We are doing exactly what you d...
- Feb 23, 2010
by
dyoungquist
Agree with what has been said so far. Check with your end c...
- Feb 24, 2010
by
DRT
Thanks for the input! We are doing a few protos this week an...
- Feb 24, 2010
by
Vince
Hi Vince,
we don't know, which kind of flux no-clean was us...
- Feb 24, 2010
by
XPS
I apologize for being so vague. It is a standard leaded proc...
- Feb 24, 2010
by
Vince
Sorry, but I don't know this brand.
Anyway pay attention, b...
- Feb 25, 2010
by
XPS
We use the OM-5100 and wash it with relatively good results....
- Feb 25, 2010
by
jdumont