Hello Sir. Our customer asked me why the solder did not co... - Mar 03, 2010 by Jeong Ju-young
The picture shows that the heel of the device lead is not on... - Mar 03, 2010 by Graham
I agree with Graham. What isn't clear is the cause; Was th... - Mar 03, 2010 by isd.jww
Hello Graham Copper. Thanks for yr comment. I will review t... - Mar 03, 2010 by Jeong Ju-young
If your "engineer reviewed the reflow profile and said this ... - Mar 03, 2010 by davef
Hi, Do you have a picture on one of these leads where the s... - Mar 05, 2010 by Graham
Ya, that could be happened bcoz of reflow profile.I think, i... - Mar 05, 2010 by Jacki
Are both photocouplers exactly the same ? More importantly... - Mar 05, 2010 by Graham
Hello Guys. Many thanks for your interest in this matter. ... - Mar 05, 2010 by Jeong Ju-young
Unfortunately, what you are calling a good fillet is not a g... - Mar 06, 2010 by isd.jww
Hi, I fully agree with isd.jww. The difference in the solde... - Mar 08, 2010 by Graham
IPC also states that side overhang on a gull wing of 50% is ... - May 17, 2010 by qaguy