We have encountered high percentage of pin holes issue after... - Mar 09, 2010 by JOSEPH
Hello Sir. We also encountered the same pin-hole issue but ... - Mar 10, 2010 by Jeong Ju-young
Hi, blow holes / pin holes / holes in joints are usually a s... - Mar 11, 2010 by Graham
Hi , Looking at your photo....can I also see a hole in the m... - Mar 11, 2010 by Graham