Hi all, lately ofen I have problem with cracked ceramic cap... - Jun 19, 2010 by iv40
Please describe the location and appearance of the crack ... - Jun 19, 2010 by davef
check your de-panelling process if you are using break-out t... - Jun 21, 2010 by orlando
Dennis: These "terminal detach failures" probably are cause... - Jun 22, 2010 by davef
Hi, about location - components are in the diferent locat... - Jun 23, 2010 by iv40
Thanks, Dennis. That is a good idea, but I have problem :... - Jun 25, 2010 by iv40
> Thanks, Dennis. That is a good idea, but I > have... - Jun 25, 2010 by Flipit
*** silly question deleted, there are no 100nF NPO *** ... - Jun 27, 2010 by leadthree
Is the board a two sided smt board? If so, where are the sta... - Jul 06, 2010 by Baildl632
A couple of things: Does the cap break if you try to remo... - Jul 09, 2010 by Reese
I had cracking caps from the ICT and a variation in the leng... - Jul 12, 2010 by leadthree