Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6088
I need a second opinion. My operators us an air hose to ... - Nov 04, 2010 by floydf
You got my vote. I would not want to be on the other side o... - Nov 04, 2010 by SteveO
It would depend on the solder paste but the stuff we use is ... - Nov 04, 2010 by iddgmbj
The smallest particle sixe for type 3 paste in 25 microns. ... - Nov 05, 2010 by Mark
I agree with the others - I just don't see the danger. We'v... - Nov 05, 2010 by ScottE
What about trying to clean these stencils with a proper sten... - Nov 05, 2010 by SMTSales
I think you are right. According to IPC-7526 section 6.2 say... - Nov 05, 2010 by DeanM
I agree that the tines (webs between apertures) can become d... - Nov 05, 2010 by Chartrain
I would also be concerned about spreading solder paste on th... - Nov 12, 2010 by Dick