Views: 10355
Hello guys !
I have a problem, I am finding some blow h...
- Jan 12, 2011
by
Armando_Gomez
How many % were affected?
If a few,it can be caused bcoz of...
- Jan 12, 2011
by
Jacki
We've never seen the defect that you describe, but in wave s...
- Jan 13, 2011
by
davef
Hi I hope this pictures helps
this is the link
...
- Jan 20, 2011
by
Armando_Gomez
Armando
Link does not work. Goes to a "page not found" e...
- Jan 20, 2011
by
dyoungquist
www.flickr.com/photos/ ...
- Jan 21, 2011
by
Armando_Gomez
Hi,
in my experience, the humidity is trapped in the solder...
- Jan 21, 2011
by
XPS
Try baking your boards first to remove the moisture. Moistur...
- Jan 21, 2011
by
aci
Hi
In my experience try to change component to another batc...
- Jan 23, 2011
by
Piter
Hello!
I've had the same problem about one Jear ago. We h...
- Jan 24, 2011
by
Fönsi