Hi,
We are using ws488 sn100c paste.
Anyone have a pr...
- Mar 30, 2011
by
gaz
While you're waiting, consider giving your paste manufacture...
- Mar 31, 2011
by
robgd3
starting point with zone settings would be, 100 / 160 / 200 ...
- Apr 01, 2011
by
Graham
This VIP70 has thermocouple inputs, so I'm hoping that's a...
- Apr 04, 2011
by
gaz
one of my customers with a BTU VIP 70 has the following sett...
- Apr 05, 2011
by
Graham
That's very helpful, and much appreciated.
I know it's ...
- Apr 05, 2011
by
gaz
It is one of our pastes...Almit LFM48 W TM-HP, a high reliab...
- Apr 05, 2011
by
Graham
We are not having any real issues. I am just first setting...
- Apr 05, 2011
by
gaz
Almit are specialists in formulating fluxes for pastes and w...
- Apr 06, 2011
by
Graham
ok, thanks very much for your help.
...
- Apr 06, 2011
by
gaz